Home

WSC 110 · Welding Construction

Session 3 · Hour 1 · The set is the bead

Instructor cue 조건이 비드다.

90 minNow Open · 5 min left · next Demo

Set the heat. Hold the length.

0/6

  • Too many amps. Undercut and spatter.

  • Too few amps. Lack of fusion. Overlap.

  • Long arc. Unstable. Spatter. Dirty metal.

  • Weave two to three rod diameters. Then split the pass.

  • Hot start at the beginning. Fill the crater at the end.

  • Carbon to stainless. Butter with 309. Stick, not SAW.

CheckHold arc length to the rod. Name the 309 butter. SAW is out. Arc ≈ rod. Butter named. SAW refused.