TIG 110 · TIG Mild Steel Butt
Session 3 · Hour 1 · Watch the pool
Instructor cue 아크는 시계가 아니다.
90 minNow Open · 5 min left · next Demo
CheckClean the plate. Confirm argon. A test arc. A straight bead. Filler if the paper asks. Write width, ripple, oxide. Do not invent amps. Same current, different hands. The walk is the weld. A dip means grind, then start honest.